What air content is required for concrete on Washington DOT projects?

"Air content for concrete Class 4000D shall conform to Section 6-02.3(2)A1. For all other concrete, air content shall be a minimum of 4.5 percent and a maximum of 7.5 percent for all concrete placed above the finished ground line unless noted otherwise." [1] "a. The concrete shall maintain an air content between 4.5 and 7.5 percent." [1] "Commercial concrete placed above the finished ground line shall be air entrained and have an air content from 4.5 percent to 7.5 percent in accordance with FOP for AASHTO T 152." [2] "Air content shall be tested in accordance with WSDOT Test Method T 818, and shall conform to Section 6-02.3(2)A." [2] "Air content shall conform to Section 6-02.3(2)A." [2] "the lower Specification limit for Air Content shall be 3 percent, and the upper Specification limit for Air Content shall be 7 percent." [3] "The lower Specification limit for air content shall be 3 percent, and the upper Specification limit for air content shall be 7 percent." [3]

Every answer carries its source — tap a citation to read the official document.

This answer came from Verika — an expert in your pocket. Ask anything, out loud or typed; answers come from your region’s regulations and your team’s own knowledge, cited to the source. If it isn’t in the sources, Verika says so.

Verika provides information with citations to help you find and understand the rules that apply to your work. It is not a substitute for professional engineering or legal judgment. Answer generated 2026-08-28; always confirm against the cited source for your project.

More Washington answers